#4 from wax to bronze- Preparing the shell for casting in bronze
24hrs. after the last dip of the shells we cut off the tops of the cups.
Then we cut slits in the shell to keep them from cracking when the wax heats and expands.
These shells are then put in the kiln cup side down and heated.
The wax runs out of the shells into a bucket under the kiln. This is the lost wax casting method.
Once the empty shells have cooled we patch any cracks and all the cuts used to release the wax except the cup opening and the two main vents that exit at the top of the cup.